1.Lignosulfonate superplasticizer dosage of cement content 0.20-0.30%, commonly used dosage is 0.25% water reduction of up to 9-11%. In the appropriate dosage when compared with the reference concrete strength increased by 15-20% 3 days, 7 days strength increased 20-30%, 28 days by 15-20%, long-term strength also increased.
2.Without changing the water in the case of concrete( suggested ratio 0.65)1to increase the flow of concrete, improved work-ability.
3.In keeping concrete slump, the same intensity and the reference concrete, cement can save 8-10%, the use of one ton of Lignosulfonate superplasticizer powder, can save 30-40 tons of cement.
4.In the standard state, concrete mixed with this agent may delay compared with the reference concrete setting time of concrete more than 3 hours, the final setting time of 3 hours, the peak heat of hydration delayed more than five hours, is conducive to summer construction and commodity concrete transport and mass concrete.
5.Lignosulfonate superplasticizer with micro-entraining, can improve the impermeability of concrete freeze-thaw performance.
6.After the agent mixed concrete and aggregates of reinforced non-corrosive.
7.Increase its water dispersion capacity to avoidwater bubble inside the slump.